No | Ink Type | Substrate To Be Printed | Reducer | Remark |
1 | DN | Non treated PP Treated PP, PE | Solvent 631 30 – 50% (Toluene:IPA:EA=6:3:1) | Disadvantage : Low heat resistance (not more than 1000C) Oil resistance is very bad |
2 | DN Re-3 | HDPE Film | Solvent 631 ± 50 % | Characteristic : Good crincle & scratch resistance Disadvantage : Inferior gloss compared with the other type |
3 | DC | Paper, Board, Al-foil | Solvent 631 ± 50 % | Characteristic : High heat resistance (± 2000C) |
4 | TM | Treated PP | Toluene ± 50 % | Characteristic : Good oil resistance |
5 | TX | Treated PP | Toluene ± 30 % | Characteristic : Oil resistance is very bad, low price. |
FOR REVERSE PRINTING
No | Ink Type | Substrate To Be Printed | Reducer | Remark |
1 | LPPL | Treated O P P | Toluene + EA ± 40 % | For PE Extrusion Laminating / Dry Laminating / Metallizing Overprint by Anchor Coating Agent before laminating |
2 | LX-01 | Treated PET | Toluene + EA ± 40 % | For PEEL / Dry Laminating / Metalilizing Overprint by Anchor Coating Agent before laminating |
3 | LX-02 | Treated OPP | Toluene + EA ± 40 % | For PP Extrusion Laminating : Anchor Coating is not necessary For PEEL/Dry Laminating/ Metallizing: use Anchor Coating Agent |
4 | DC | Cellophane film | Solvent 631 ± 50 % | For PEEL : Use Anchor Coating Agent |
5 | VA | Shrinkable PVC | Solvent 631 ± 50 % | Characteristic : High heat resistance |